Hi guys, I have a question...

On my Miller 350LX with the pulser on(mind you, first tig machine I have run with pulse), on .125" 5086 Al, 140 amps and the pulser set at 50% on the back ground amps, 2 pps, 50% peak time, why do the welds look frosty?

I have tried adjusting the back ground,...